Blog

Running a Rover in Winter: Batteries, Traction and Electronics Below Freezing

Tom Cosgrove,

Reading Room: The Fictionlab Blog

TL;DR: Cold weather robot operation fails in three predictable ways: usable battery capacity drops, wheels lose grip on compacted snow and ice, and condensation can form inside electronics during temperature transitions. None of these are mysterious. Lithium-ion cells lose both capacity and available discharge power as temperature falls, and charging a Li-ion pack below 0 °C risks lithium plating, so you warm the pack first. Traction is a function of contact patch, tread geometry and wheel torque control, not raw motor power. Condensation commonly happens when you move a cold robot into a warm room, rather than while it sits outside. The fix for all three is procedural: plan shorter mission windows, keep batteries warm until the moment of use, derate your payload, and seal or acclimatize electronics before transitions. The Leo Rover and Raph Rover official operating temperature ranges should be checked in their datasheets before any sub-zero deployment – do not assume room-temperature specs hold in the field.

Why Does Cold Weather Robot Operation Break Mission Plans?

A mobile robot that works reliably at 20 °C can behave very differently at -10 °C. The failure modes are rarely dramatic. More often, the robot simply does less: shorter runtime, slower acceleration, intermittent sensor dropouts, a wheel that spins instead of climbing a ramp. Each of these is individually tolerable. Combined, they turn a 90-minute inspection route into a 35-minute partial survey and a recovery walk.

Cold weather robot operation is a systems problem. The battery, drivetrain, enclosure and compute stack all degrade along different curves, and they interact. A battery delivering less voltage under load can require higher battery current to maintain the same mechanical output, which generates some internal heat and may improve performance slightly. Meanwhile the same cold that hurts the battery stiffens tire rubber and reduces its coefficient of friction on ice, so the drivetrain demands more torque than it would in summer. The system finds a new equilibrium, usually a worse one.

This guide covers four areas where field teams lose time in winter: battery behavior and charging, traction on snow and ice, condensation and electronics, and pre-mission preparation. The focus is on mechanisms and procedures you can apply to any UGV, with notes specific to Fictionlab platforms where the hardware design matters.

How Much Battery Capacity Do You Actually Lose Below Freezing?

Lithium-ion chemistry slows down when it gets cold. The electrolyte becomes more viscous, lithium-ion diffusion through the electrode material slows, and internal resistance rises. Two separate effects follow, and conflating them is a common planning error in cold weather robot operation.

Capacity loss versus power loss

Capacity loss is how many amp-hours the pack can deliver before hitting cutoff voltage. Power loss is how much current the pack can supply at any instant without the voltage sagging below the controller’s brownout threshold. Power loss is usually the more severe effect at moderate cold, and it is the one that causes surprise shutdowns under peak load – climbing a curb, breaking free from a snow drift, or spinning up all four motors simultaneously.

Published cell datasheets from major Li-ion manufacturers typically characterize discharge at -20 °C, 0 °C, 25 °C and 60 °C. Consult the datasheet for your specific cell chemistry rather than relying on a general rule of thumb. The qualitative pattern is consistent across cylindrical Li-ion cells: usable capacity at 0 °C is meaningfully below the 25 °C rating, and at -20 °C the reduction is substantially larger, with a further drop when discharge rate is high. Treat any single percentage figure you find online with suspicion unless it names the cell and the discharge rate.

For mission planning, the practical approach is empirical. Run your actual robot, with your actual payload, on your actual route, at the temperature you expect. Log pack voltage and current. That measured runtime is your plan. Do not scale a summer figure by a borrowed percentage.

Why you must not charge a cold lithium pack

This is the single hardest constraint in cold weather robot operation, and it is a safety issue rather than a performance one. Charging a lithium-ion cell below approximately 0 °C can cause lithium plating: metallic lithium deposits on the anode surface instead of intercalating into the graphite. The deposits are permanent, they reduce capacity, and over repeated cycles they can form dendrites that eventually short the cell internally. The result is accelerated degradation at best and a thermal event at worst.

Well-designed battery management systems enforce a low-temperature charge cutoff. If your BMS does, it will simply refuse the charge, which looks like a broken charger to a cold, frustrated operator in a field van. If your BMS does not enforce this, you are responsible for enforcing it. The procedure is straightforward.

Before charging any Li-ion pack that has been in sub-zero conditions, follow these steps:

  • Bring the pack into a heated space and let it equilibrate to above 0 °C throughout, not just on the surface. A large pack can take well over an hour.
  • Measure cell or pack temperature if your BMS exposes it over the telemetry interface. Do not estimate from ambient air.
  • Allow any surface condensation to evaporate fully before connecting the charger.
  • Follow the battery manufacturer’s permitted charging temperature and charge-rate limits. If charging near the low end of that range is permitted, use a reduced rate if your charger supports it.

Discharging below 0 °C is generally permitted by cell datasheets, often down to -20 °C, but with the reduced performance described above. Charging is the hard limit. Keep the two rules separate in your head and in your field checklist.

Practical battery handling in the field

The most effective battery strategy for winter work is thermal: keep the packs warm until the moment they enter service. Store spares in an insulated case inside a heated vehicle. Swap in a warm pack rather than nursing a cold one. A pack that starts the mission at 20 °C and generates heat from its own internal resistance during operation will usually outperform an identical pack that started at -15 °C, even in the same ambient conditions.

A robot in motion generates waste heat in the motors, drivers and battery itself. If the battery compartment is reasonably insulated, this self-heating can be a real effect. It argues against long idle periods during a winter mission: a robot parked for twenty minutes while an operator reviews imagery will restart colder and weaker than one that kept moving.

What Determines Traction on Snow and Ice?

Traction is the product of normal force and the coefficient of friction at the contact patch. In winter you can lose on both terms, and the loss is not uniform across surfaces.

Surface types behave very differently

Lumping “winter conditions” into one category causes planning failures. The relevant distinctions for a wheeled UGV are these:

  • Fresh dry snow compacts under the wheel and can offer reasonable shear strength. Deep fresh snow becomes a clearance problem rather than a friction problem – the chassis belly starts bulldozing.
  • Compacted snow is firm and generally manageable, with a coefficient of friction well below dry asphalt but usable with appropriate tread.
  • Wet snow near 0 °C can form a water film at the contact patch. This is significantly more slippery than dry snow and it packs into tread voids, effectively turning a treaded tire into a slick.
  • Black ice is the worst case. The coefficient of friction between rubber and smooth ice near 0 °C is very low, and tread pattern helps little because there is little for the tread blocks to bite into.
  • Frozen rutted ground can be high-friction but geometrically hostile. The failure mode is wheel lift and loss of contact, not slip.

Tread, rubber and contact patch

Rubber compounds stiffen as temperature falls. A tire optimized for summer grip loses conformability in the cold, reducing the micro-scale interlocking that produces friction on rough surfaces. This is why automotive winter tires use softer compounds with a lower glass transition temperature. The same physics applies to robot tires, though the compound choice available on small-diameter wheels is usually limited.

What you can control more easily is tread geometry and contact patch. Open tread with large voids helps clear snow and reduce packing. A wider contact patch lowers ground pressure, helping on soft snow where the failure mode is sinking, but it does not necessarily help on ice where the failure mode is shear. These two goals conflict, which is why there is no universal winter wheel.

The Leo Rover uses a four-wheel-drive layout with independently driven wheels, which matters in snow for a specific reason: when one wheel loses grip, the remaining three can still contribute tractive effort if the control scheme limits torque to the slipping wheel. An open mechanical differential can limit axle torque when one wheel slips. Independent motor drive avoids that specific mechanical coupling, although it does not create traction where the remaining wheels have insufficient grip.

Controlling slip rather than fighting it

Raw torque does not produce traction beyond the friction limit. Once a wheel exceeds the slip ratio at which friction peaks, applying more torque makes things worse – the wheel spins, polishes the ice, and can heat a thin water film that reduces grip further.

If you are running ROS 2 on the platform, you have the tooling to address this in software. Practical measures include limiting commanded acceleration in the velocity controller, comparing wheel odometry against an IMU-derived velocity estimate to detect slip, and reducing torque on wheels whose encoder-reported speed diverges from the chassis estimate. None of this requires exotic hardware. It requires that your control loop runs fast enough to react before the wheel has spun up, and that your odometry source is independent of the wheels you are trying to regulate.

Be aware that wheel odometry becomes unreliable in winter. Slip corrupts the dead-reckoning estimate in a way that is often biased rather than random – the robot may consistently think it has traveled farther than it has. If your navigation stack fuses wheel odometry with IMU and an exteroceptive source such as LiDAR or visual odometry, increase the covariance you assign to the wheel source in cold conditions. A mis-tuned fusion filter that trusts slipping wheels will drift badly.

How Does Condensation Damage Electronics, and When Does It Form?

Condensation is one of the most misunderstood winter risks in cold weather robot operation. Operators worry about it while the robot is outside in the cold. Under stable outdoor conditions, that is usually not when it happens.

The physics of the transition

Condensation forms when a surface is colder than the dew point of the surrounding air. Outdoors in winter, the air is cold and holds little absolute moisture, and the robot is often at roughly the same temperature as the air. There is usually no strong driver for condensation, although frost or condensation can still occur during rapid weather changes, fog or radiative cooling.

The danger is often the transition into a warm environment. Bring a robot that has been at -10 °C into a heated workshop at 20 °C with 50% relative humidity, and exposed cold surfaces can be well below the room’s dew point. Water can condense on circuit boards, connectors and camera lenses. Moisture can also form inside an enclosure if humid air can enter it or was already trapped inside. Powering the robot on in that state risks shorts and corrosion.

The reverse transition matters too. If warm, humid air is trapped inside an enclosure and the robot is then cooled outdoors, its moisture can condense inside the enclosure. This is why outdoor enclosures are often assembled in dry conditions or include desiccant.

Procedures that actually work

Three approaches handle condensation, and they can be combined.

  1. Acclimatize before opening or powering on. Bring the robot indoors and leave it sealed and powered off for a period long enough for the whole mass to reach room temperature. For a platform with a substantial aluminum chassis and battery, plan on a couple of hours rather than twenty minutes. Thermal mass is what sets the timescale.
  2. Control enclosure humidity. An enclosure with a verified ingress protection rating can limit direct water ingress, while internal desiccant packs can reduce trapped humidity. Check the desiccant’s color indicator regularly and regenerate or replace it when saturated; a saturated pack no longer provides useful moisture absorption.
  3. Use a breathable vent where appropriate. A Gore-type pressure-equalization vent lets the enclosure equalize pressure during thermal cycling while resisting liquid-water ingress. Such vents pass water vapor, so they do not replace humidity control or desiccant inside the enclosure.

Beyond condensation, two other cold effects deserve attention. Lens fogging on cameras degrades vision-based perception and often appears exactly when the robot drives from a cold outdoor area into a warmer indoor one – a common pattern in inspection work that crosses building thresholds. Some camera modules include small heaters for this reason. Separately, LCD displays and some MEMS sensors have narrower rated temperature ranges than the processors they support, so the limiting component in your stack may not be the one you expect. Check every datasheet in the payload chain, not just the compute board.

What Should Your Pre-Mission Winter Checklist Include?

Most winter failures are preventable with preparation rather than hardware changes. The checklist below separates the steps by when they happen, because timing matters as much as content.

The day before

Preparation work that cannot be done in the field belongs here:

  • Charge all packs to full at room temperature and verify cell balance through the BMS if your platform exposes that telemetry.
  • Inspect tires for cracking and confirm tread is appropriate for the expected surface. Swap wheels if you have a winter set.
  • Check and replace desiccant in sealed enclosures.
  • Verify cable strain reliefs and connector seals. Cold makes plastics brittle and insulation stiff, so a marginal cable fails in winter before it fails in summer.
  • Update and test your ROS 2 software stack indoors. Debugging a launch file at -10 °C with gloves on is not a good use of a field day.

At the site

Field procedure should keep thermal management front of mind:

  • Keep batteries in an insulated case in a heated vehicle until the moment of installation.
  • Power on and allow time to complete startup checks before commanding motion. This surfaces startup faults while the robot is still within reach.
  • Run a short known test route before committing to the full mission. Compare observed current draw and odometry drift against your baseline.
  • Derate the planned mission by a meaningful margin. If summer runtime is 120 minutes, do not plan a 110-minute winter route.
  • Avoid unnecessary idle time, which allows the battery and drivetrain to cool.
  • Plan a recovery path. Assume the robot may stop at the farthest point of the route and confirm you can physically reach it.

After the mission

The post-mission steps protect the hardware for the next deployment:

  • Do not charge cold packs. Bring them indoors and let them reach above 0 °C before connecting a charger.
  • Let the robot acclimatize sealed and powered off before opening the enclosure or powering on indoors.
  • Once dry and at room temperature, clean road salt and grit off the chassis and wheels. Salt is corrosive and it finds its way into bearings and connector shells.
  • Download and review logs while the mission is fresh. Current draw, voltage sag under load and odometry drift are the three signals that tell you how the cold actually affected the platform.

A note on official specifications

Operating temperature ranges for Fictionlab platforms are published in the product documentation. Use those figures rather than inference. The Raph Rover and Leo Rover are different platforms with different enclosures, drivetrains and thermal characteristics, and a limit that applies to one does not transfer to the other. If a planned deployment sits near or outside the published range, treat that as a design question to resolve before the field day, not a limit to discover during it.

Frequently Asked Questions

Can you charge a robot battery outdoors in winter?

Not if the pack is below approximately 0 °C, unless its manufacturer explicitly permits charging at that temperature. Charging a cold lithium-ion cell risks lithium plating, which permanently reduces capacity and can create internal short circuits. Bring the pack somewhere warm, let it equilibrate throughout its mass, and only then connect the charger. Many battery management systems block low-temperature charging automatically, but you should not rely on that without confirming it.

How much runtime should you expect to lose in cold weather robot operation?

It depends on cell chemistry, discharge rate, insulation and starting pack temperature, so there is no single reliable number. The honest approach is to measure it: run your configured robot on a representative route at the expected temperature and log pack voltage and current. Use that measurement for planning. Published cell datasheets for your specific battery give the discharge curves at different temperatures and are the right reference point.

Does heating the battery pack help, and is it worth the energy cost?

Yes, warming helps, and the energy accounting can favor it. A warm pack has lower internal resistance, delivers more usable capacity and sags less under peak load. The simplest approach costs nothing in onboard energy: keep spare packs in an insulated container in a heated vehicle and install a warm pack at mission start. Self-heating from normal operation can then help maintain it, provided the robot keeps moving.

What causes condensation inside a robot enclosure?

It forms when a surface is colder than the dew point of the air touching it. In practice this commonly happens when you bring a cold robot into a warm, humid indoor space, especially if humid air can enter the enclosure or is trapped inside it. Let the robot acclimatize sealed and powered off until its whole mass reaches room temperature, then open it. Desiccant packs and pressure-equalization vents can reduce risks in enclosures that cycle through many temperature transitions, but pressure vents do not block water vapor.

Why does navigation drift more on snow?

Wheel slip corrupts wheel odometry, and the error is often biased rather than random – the robot may overestimate distance traveled. If your sensor fusion configuration assigns high confidence to wheel odometry, that bias propagates into the pose estimate. In winter, increase the covariance on the wheel odometry source and lean more on IMU and exteroceptive sensing such as LiDAR or visual odometry.

Do you need different wheels for snow and ice?

It depends on which surface dominates. Open tread with large voids helps on soft and compacted snow by clearing packed material and maintaining shear contact. On smooth ice, tread geometry does relatively little because the limiting factor is the low rubber-ice coefficient of friction rather than mechanical interlock. Wider wheels reduce ground pressure and help on soft snow but do not necessarily improve grip on ice. Match the wheel to the surface you expect most.

Which component usually sets the real temperature limit on a UGV?

Frequently it is not the main compute board. Battery charge limits, LCD displays, some MEMS sensors and certain camera modules carry narrower rated temperature ranges than the processor. Check the datasheet for every component in the payload chain, including sensors and peripherals you added yourself, rather than assuming the platform’s headline figure covers the whole system.

Take the Next Step

Winter deployments reward preparation far more than they reward hardware upgrades. Keep packs warm, respect the charging temperature limit, match wheels to the actual surface, manage temperature transitions deliberately, and derate your mission plan. Most cold weather robot operation failures trace back to one of those five.

If you are evaluating a platform for field work that extends into winter conditions, review the hardware specifications, documentation and official operating temperature range for the Leo Rover and see whether its open ROS 2 architecture fits the control and sensing changes your sub-zero missions will need.


Read more